Many thanks for the suggestions. We'll check them.
Are you spin-casting the catalyst solution onto the quartz substrate
surface? High shear always helps.
We thought about using spin coating, but our solution is extremely
non-viscous, so we think it wouldn't help so much.

Jordi Riu
Dept. Analytical and Organic Chemistry
University Rovira i Virgili of Tarragona
Catalonia - Spain
Uncle Al
2004-04-01 15:50:14 UTC
Permalink
Post by Jordi Riu
Many thanks for the suggestions. We'll check them.
Are you spin-casting the catalyst solution onto the quartz substrate
surface? High shear always helps.
We thought about using spin coating, but our solution is extremely
non-viscous, so we think it wouldn't help so much.
Thicken it with a soluble polymer (viscous during shear) or maybe 1%
fumed silica plus sonication to fully disperse (not viscous during
shear - though the time evolution of non_newtonian viscosity will be
interesting).

Adding fumed silia is a good experiment in any case. Did you ever
plant a flowerbed of very small seeds (e.g., Amaranthus)? You mix the
seeds with fine sand to get easy good dispersal.
--
Uncle Al
http://www.mazepath.com/uncleal/
(Toxic URL! Unsafe for children and most mammals)
"Quis custodiet ipsos custodes?" The Net!
Ceraboy
2004-04-02 21:45:09 UTC
Permalink
Post by Jordi Riu
Many thanks for the suggestions. We'll check them.
Are you spin-casting the catalyst solution onto the quartz substrate
surface? High shear always helps.
We thought about using spin coating, but our solution is extremely
non-viscous, so we think it wouldn't help so much.
Jordi Riu
Dept. Analytical and Organic Chemistry
University Rovira i Virgili of Tarragona
Catalonia - Spain
First you need to disperse your particles better. With metal
nanoparticles, using aqueous solutions is very difficult even with
some of the best ammonium polymethacyrlate type dispersants or
electrostatic methods. Your organic solvents should work well though.
If you want to stick with methanol try some of the traditional powder
processing dispersants (ie menhaden fish oil or hypermer KD1 (made by
ICI surfactants)). You should only need less than a weight % to make
a significant improvement. Disolve your dispersant (polymer) in
solution, add your nanoparticles and disperse with an ultrasonic
probe. I have had good success dispersing carbon nanotubes in
toluene, etoh, and MEK with the fish oil in this manner. Remember if
you have good dispersion, you will not be able to see particles or
colloids with the eye. The solubility of the fish oil is improved
with about 20-40%xylene in meoh or etoh allowing the polymer chains to
stretch out and improve the steric barrier.

To thicken your solution for spin casting add some ethyl cellulose
(49% + ethoxyl content) until desired consistency is achieved
(approximately 10wieght% yields the viscosity of maple syrup).
Polyvinylbutyral works well too, but you might need a bit more to
reach equivalent viscosity of the ethyl cellulose. Further, if
absolutely clean burnout is required, use polypropylene carbonate
(trade name QPAC-40), this is the absolutely cleanest binder for
burnout which decomposes in air, vacuum, or inert. Of course you will
need to work with acetone or MEK solutions for decent solubility which
should also disperse your particles with the fish oil.

Yet one more final option is too use a higher viscosity solvent.
Alpha terineol is wonderful with a little oleic acid for the
dispersant. The alpha terpineol dries very slow, but levels
beautifully, and is quite non-toxic compared to other solvents. If
you need more body for spin coating, a % or so of ethyl cellulose will
do the trick.

Good luck
Milton Lima
2004-04-08 12:59:41 UTC
Permalink
Bon dia Jordi:


One possible hi-tech solution is to induce photofragmentation though a
high-power visible light laser. It really works !
Hello to everybody,
we are synthesizing carbon nanotubes, and our catalyst is a mixture of Fe/Mo
supported by Al nanoparticles (we do this by mixing the Fe and Mo compounds
with the Al nanoparticles in a methanol solution). We place then a microdrop
of the liquid over a quartz surface, we leave it at 170 C degrees for 5' in
order to dry the solvent and then we run the CVD process.
To avoid the formation of aggregates of catalyst and to have 'real'
nanoparticles of catalyst over all the quartz surface, we leave the
Fe-Mo-Al-methanol catalyst solution to 24 hours of magnetic rinse and then
to 2 hours of ultrasounds, just before placing the microdrop of the catalyst
mixture over the quartz surface. Despite doing this, we find some areas
where we have strong aggregates of catalyst. Does anybody have any idea in
order to avoid the formation of these aggregates of catalyst?
Many thanks in advance,
Jordi Riu
Dept. Analytical and Organic Chemistry
University Rovira i Virgili of Tarragona
Catalonia - Spain